Use este identificador para citar ou linkar para este item:
https://repositorio.ufpe.br/handle/123456789/64050
Compartilhe esta página
Registro completo de metadados
Campo DC | Valor | Idioma |
---|---|---|
dc.contributor.advisor | MERGULHÃO, Viviane Afonso | - |
dc.contributor.author | SANTOS, Maria Clara Almeida dos | - |
dc.date.accessioned | 2025-07-02T18:19:11Z | - |
dc.date.available | 2025-07-02T18:19:11Z | - |
dc.date.issued | 2025-04-01 | - |
dc.date.submitted | 2025-07-02 | - |
dc.identifier.citation | SANTOS, Maria Clara Almeida dos. Resistência à fratura de molares restaurados com diferentes materiais endocrown.2025. Trabalho de conclusão de curso (Odontologia)- Universidade Federal de Pernambuco, Recife,2025. | pt_BR |
dc.identifier.uri | https://repositorio.ufpe.br/handle/123456789/64050 | - |
dc.description.abstract | Dentes tratados endodonticamente são mais propensos a falhas biomecânicas, tornando essencial o reforço com um material restaurador que possua boas propriedades mecânicas. Este estudo avaliou a resistência à fratura e o padrão de falha de molares restaurados com diferentes materiais endocrown. Quinze molares inferiores tratados endodonticamente foram divididos em três grupos (n=5). G1: Endocrown de dissilicato de lítio; G2: Endocrown de zircônia; G3: Coroa de dissilicato de lítio com núcleo de resina composta (grupo controle). As amostras foram cimentadas adesivamente (cimento resinoso All Cem Core / FGM). Pino de fibra White Post DC foi utilizado (grupo controle). As amostras foram submetidas a envelhecimento artificial e posteriormente a uma carga compressiva sobre a superfície oclusal da restauração, a uma velocidade de 1 mm/min até ocorrer a fratura. As amostras fraturadas foram analisadas para determinar o padrão de fratura utilizando um estereomicroscópio. O teste não paramétrico de Kruskal-Wallis foi utilizado para comparar a resistência à fratura entre os grupos, e os resultados dos padrões de fratura foram analisados pelo teste exato de Fisher (α=0,05). As médias (desvio padrão) das cargas de falha (N) para os grupos foram as seguintes: G1: 1659,7 (695,4); G2: 2876,3 (983,4); G3: 3096,0 (694,8). O teste de Kruskal-Wallis não revelou diferenças significativas entre os grupos (p > 0,05). Em relação aos padrões de fratura (catastrófica x reparável), não foi observada diferença significativa (p > 0,05) entre os grupos. Concluiu-se que restaurações do tipo endocrown cerâmica demonstram desempenho mecânico adequado e resistência à fratura comparável à das coroas cerâmicas convencionais, podendo, portanto, ser consideradas uma alternativa atrativa para restaurar molares tratados endodonticamente. | pt_BR |
dc.format.extent | 39 p. | pt_BR |
dc.language.iso | por | pt_BR |
dc.rights | embargoedAccess | pt_BR |
dc.rights.uri | https://creativecommons.org/licenses/by-nc-nd/4.0/ | pt_BR |
dc.subject | Resistência à fratura | pt_BR |
dc.subject | CAD-CAM | pt_BR |
dc.subject | Endocrown | pt_BR |
dc.title | Resistência à fratura de molares restaurados com diferentes materiais endocrown | pt_BR |
dc.type | bachelorThesis | pt_BR |
dc.degree.level | Graduacao | pt_BR |
dc.contributor.advisorLattes | http://lattes.cnpq.br/1990352272679721 | pt_BR |
dc.description.abstractx | Endodontically treated teeth are more prone to biomechanical failures, making reinforcement with a restorative material with good mechanical properties essential. This study evaluated the fracture resistance and failure mode of molars restored with different endocrown materials. Fifteen endodontically treated mandibular molars were divided into three groups (n=5). G1: Lithium Disilicate Endocrown; G2: Zirconia Endocrown; G3: Lithium Disilicate Crown with Composite Resin Core Build-up (control group). Specimens were adhesively cementely (All Cem Core resin cement /FGM). White Post DC fiber post (control group) was used. The specimens were subjected to artificial aging and subsequently to a compressive load on the occlusal surface of the restoration at a crosshead speed of 1 mm/min until fracture. The fractured specimens were analyzed to determine the fracture pattern using a stereomicroscope. The non-parametric Kruskal-Wallis test was used to compare fracture resistance of the groups and the results of fracture patterns were submitted to the Fisher exact test ( α=0.05). Mean (standard deviation) failure loads (N) for groups were as follows: G1: 1659.7 (695.4); G2: 2876.3 (983.4); G3: 3096.0 (694.8). Kruskal-Wallis test did not reveal significant differences between groups (p > 0.05). Regarding fracture patterns (catastrophic x repairable), no significant difference (p > 0.05) was observed among the groups. It was concluded that ceramic endocrown restorations demonstrate adequate mechanical performance and fracture resistance comparable to that of conventional ceramic crowns, and can therefore be considered an attractive alternative for restoring endodontically treated molars. | pt_BR |
dc.subject.cnpq | Áreas::Ciências da Saúde | pt_BR |
dc.degree.departament | ::(CCS-DPCB) - Departamento de Prótese e Cirurgia Buco Facial | pt_BR |
dc.degree.graduation | ::CCS-Curso de Odontologia | pt_BR |
dc.degree.grantor | Universidade Federal de Pernambuco | pt_BR |
dc.degree.local | Recife | pt_BR |
Aparece nas coleções: | (TCC) - Odontologia |
Arquivos associados a este item:
Arquivo | Descrição | Tamanho | Formato | |
---|---|---|---|---|
TCC Maria Clara Almeida dos Santos.pdf Item embargado até 2026-07-03 | 5,21 MB | Adobe PDF | Visualizar/Abrir Item embargado |
Este arquivo é protegido por direitos autorais |
Este item está licenciada sob uma Licença Creative Commons